Inoculant #SDBH-Silicon(0.7-3)
Description
Ductile cast iron special · CV cast iron
Pinhole and scum defect preventive inoculants
Silicone addition for extremely low Al molten iron
Pinhole and scum defect preventive inoculants
Silicone addition for extremely low Al molten iron
Feature
Aiming at and preventing various casting defects of ductile iron, especially to prevent
① Hydrogen system pinhole defects
② Defects of slag inclusion (oxide scum)
The manufactured high-performance ductile iron, CV cast iron special low Al, low scum, casting defect prevention type inoculation agent.
① Hydrogen system pinhole defects
② Defects of slag inclusion (oxide scum)
The manufactured high-performance ductile iron, CV cast iron special low Al, low scum, casting defect prevention type inoculation agent.
Effect
◎ Low Al, low dross, easy to dissolve, few impurities, so the defects of dross (oxide dross) are reduced.
◎ It can prevent the hydrogen-based pinhole defects in the ductile iron of small parts and thin parts.
◎ Improve the number of graphite particles.
◎ When used in low-Al molten iron, it can extend the life of the induction furnace and simplify the slag removal work
◎ It can prevent the hydrogen-based pinhole defects in the ductile iron of small parts and thin parts.
◎ Improve the number of graphite particles.
◎ When used in low-Al molten iron, it can extend the life of the induction furnace and simplify the slag removal work
Chemical
Si: 75%
Al: 0.3%
Ca: 0.3%
Al: 0.3%
Ca: 0.3%
Size
0.7~3㎜
3~10㎜
3~10㎜
Pack
20kg/bag
500kg/bag
1 ton/bag
500kg/bag
1 ton/bag
Use
FCD applicable
Other
◎ Effective when added after spheroidization. At the same time it can be bred.
◎ Because it is very easy to dissolve, it can be thrown in one time, or it can be added in the process of molten iron flowing. It has good effect.
◎ When inoculated in the treatment pot, the standard addition rate is 0.2% to 0.5%.
(The figures for the amount of molten iron)
◎ Adding 1% of SDBH inoculant, Si increased by 0.75%.
◎ Because it is very easy to dissolve, it can be thrown in one time, or it can be added in the process of molten iron flowing. It has good effect.
◎ When inoculated in the treatment pot, the standard addition rate is 0.2% to 0.5%.
(The figures for the amount of molten iron)
◎ Adding 1% of SDBH inoculant, Si increased by 0.75%.